📨 Have you signed up to the Forum's new Email Digest yet? Get a selection of trending threads sent straight to your inbox daily, weekly or monthly!

Newly skimmed plaster - slight hairline cracks - painting?

Just had my walls skimmed (few weeks ago now), and whilst painting I noticed a few very minor hairline cracks. Is there anything I should do to these or just paint over them?
Debbie

Comments

  • paullwill8
    paullwill8 Posts: 488 Forumite
    Fistly make sure your first 2 coats of paint are watered down by 20% water and use matt, not silk or soft sheen. Then apply two further coats un-diluted. If the cracks are very fine and you are using a decent quality emulsion then they will dissapear.
    What goes around - comes around
    give lots and you will always recieve lots
  • misgrace
    misgrace Posts: 1,486 Forumite
    debbie42 wrote: »
    Just had my walls skimmed (few weeks ago now), and whilst painting I noticed a few very minor hairline cracks. Is there anything I should do to these or just paint over them?


    Hi debbie, is this in connection with your 'vinyl paint post', is the hairline cracks, in the bare plaster, or in hairline cracks 'crazing' in the painted plaster?
  • debbie42
    debbie42 Posts: 2,586 Forumite
    misgrace wrote: »
    Hi debbie, is this in connection with your 'vinyl paint post', is the hairline cracks, in the bare plaster, or in hairline cracks 'crazing' in the painted plaster?

    It's not crazing (phew!). It's just a couple of very fine cracks around the corner of the door frame. I noticed it before painting.

    I did sand down all the walls in the end and have just painted my first watered down coat of topcoat, yesterday. I didn't manage to sand the ceiling as well as I would have liked, as it was just too awkward. The rest wasn't as bad as I feared, with my sander, though it was very dusty!

    I'm going to leave it for a week before putting on the next (final, hopefully) coat. The finish looks good at the moment, so I'm keeping my fingers crossed.
    Debbie
  • debbie42
    debbie42 Posts: 2,586 Forumite
    paullwill8 wrote: »
    Fistly make sure your first 2 coats of paint are watered down by 20% water and use matt, not silk or soft sheen. Then apply two further coats un-diluted. If the cracks are very fine and you are using a decent quality emulsion then they will dissapear.

    Bit late for the first suggestion, but thanks anyway! I did use Matt, but unfortunately it was Vinyl.
    Debbie
  • misgrace
    misgrace Posts: 1,486 Forumite
    Hi debbie,

    Thats not too bad if there is only a few, and TBH 99% of all new plaster has hairline cracks.
    If they are fine then dont worry, just lightly sand and paint.

    A good few coats of paint will hide them, and they probably wont get any wider either, well at least not for a few years.:D
This discussion has been closed.
Meet your Ambassadors

🚀 Getting Started

Hi new member!

Our Getting Started Guide will help you get the most out of the Forum

Categories

  • All Categories
  • 351.3K Banking & Borrowing
  • 253.2K Reduce Debt & Boost Income
  • 453.7K Spending & Discounts
  • 244.2K Work, Benefits & Business
  • 599.4K Mortgages, Homes & Bills
  • 177.1K Life & Family
  • 257.7K Travel & Transport
  • 1.5M Hobbies & Leisure
  • 16.2K Discuss & Feedback
  • 37.6K Read-Only Boards

Is this how you want to be seen?

We see you are using a default avatar. It takes only a few seconds to pick a picture.